4 Kg pail
|
|
Cementitious,
passivating, antirust grout, for reinforcing iron bars treatment.
Consumption
= 0.2 Kg/m of iron bar.
|
3
kg sack + 1 kg bottle
|
|
Fibre
reinforced, thixotropic, shrink resistant mortar, with normal curing
time. It is specific for structural refurbishment, with medium and
high thickness, by machine application, of masonries and concrete
structures. It contains MuCis Migrating Corrosion Inhibitors.
Consumption
= 18-19 kg/sqm/cm.
|
25
kg sack
56 sacks pallet
|
|
Fibre
reinforced, shrink resistant mortar, having maximum thixotropy and
fast curing time (15-20 min.). It is specific for structural restorations,
against the corrosion of reinforcing bars and for a rapid finishing
of the mortar (aggregate maximum dimension 1.2 mm)
It contains MuCis Migrating Corrosion Inhibitors.
Consumption
= 18-19 kg/sqm/cm.
|
25
kg sack
56 sacks pallet
|
|
Fibre
reinforced, shrink resistant mortar, having high adhesion and resistance,
maximum thixotropy and very fast curing time (5-10 min.). against
the corrosion of reinforcing bars and for a rapid finishing of the
mortar (aggregate maximum dimension 1.2 mm)
It contains MuCis Migrating Corrosion Inhibitors.
Consumption
= 18-19 kg/sqm/cm.
|
|

|
|